FOM Name: Indenter Bruker PI85/95 Pico indenter
Model Number: Bruker PI85
Contact: Julie Morasch (morasch@wisc.edu, 608-262-3613)
Center: NIAC
Location: MSE Rm 118
The Bruker PI 95 Picoindenter is an in situ mechanical testing device that operates within the TF-30 TEM. Video capture of the TEM signal allows correlation of the images with mechanical testing results.
This is an accordion element with a series of buttons that open and close related content panels.
Instrument Configuration
- Max Force 1 mN
- Force Noise Floor <0.2 µN
- Max Displacement 1 µm
- Displacement Noise Floor <1 nm
- Feedback Control Rate 78 kHz
- Max Data Acquisition Rate 39 kHz
- Fine Sample Positioning Range XYZ 50 µm / 50 µm / 3 µm
- Fine Sample Positioning Sensitivity XYZ 2 nm / 2 nm / 0.1 nm
- Coarse Sample Positioning Range XYZ 750 µm / 750 µm / 5000 µm